Polymer Property : Tensile Modulus = 194.74 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.3427 GPa

@Temperature 30.0 °C
194.74 ksi

@Temperature 86.0 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)  (Unverified Data**)
Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part..