Polymer Property : Tensile Modulus = 1938 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 13.36 GPa
1938 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66
LNP* THERMOCOMP* RFB66 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 30% Glass Bead.
Tensile Modulus 13.36 GPa
1938 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF0069XZ PA 66
LNP THERMOCOMP* RF0069XZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant.