Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.02 GPa | 1888 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® CY-20GF/000 UV FR V0 PC/ABS Blend, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedIgnition ResistantNon-HalogenatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 13.02 GPa | 1888 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP ZF0089 PPE+PS LNP* THERMOCOMP* ZF0089 is a compound based on PPE+PS resin containing 40% Glass Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. |