Mechanical Properties Metric English Comments
Tensile Modulus 126.2 GPa

@Temperature 24.0 °C
18300 ksi

@Temperature 75.2 °F
Hexcel® HexPly® F155 Epoxy Resin, T3T095 Carbon Tape
Hexcel designation: TXX095-12"-F155; Various fibersInformation provided by HexCel