Hexcel® HexPly® F155 Epoxy Resin, T3T095 Carbon Tape

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® F155 Epoxy Resin, T3T095 Carbon Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hexcel designation: TXX095-12"-F155; Various fibersInformation provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1552 MPa

@Temperature 24.0 °C
225100 psi

@Temperature 75.2 °F
Tensile Modulus 126.2 GPa

@Temperature 24.0 °C
18300 ksi

@Temperature 75.2 °F
Compressive Yield Strength 924 MPa

@Temperature 71.0 °C
134000 psi

@Temperature 160 °F
1158 MPa

@Temperature 24.0 °C
168000 psi

@Temperature 75.2 °F
Compressive Modulus 109.6 GPa

@Temperature 24.0 °C
15900 ksi

@Temperature 75.2 °F
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.0094
Laminate
Dry Resin Content (%) 38-40
Prepreg
Fiber Volume (%) 57
Laminate
Flow (%) 4-16