Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.373 GPa | 1794.6 ksi | ISO 527 |
Ecomass® 4301ZC82 Stainless Steel Filled Polyphthalamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsStainless Steel Powder Filled Polyphthalamide (PPA)Very Good ToughnessInformation provided by Technical Po.. |