Polymer Property : Tensile Modulus = 12.373 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 12.373 GPa
1794.6 ksi
ISO 527
Ecomass® 4301ZC82 Stainless Steel Filled Polyphthalamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsStainless Steel Powder Filled Polyphthalamide (PPA)Very Good ToughnessInformation provided by Technical Po..