Tensile Modulus 12.26 GPa
1778 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Verton NV0081EV_GY7E149 PC+ABS
Preliminary data for 40% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.