Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.08 GPa | 1752 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DEL139P PC LNP* STAT-KON* DEL139P is a compound based on Polycarbonate containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: Electrically Conductive, Exceptional Processing, Flame Retar.. |