Polymer Property : Tensile Modulus = 12.08 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 12.08 GPa
1752 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DEL139P PC
LNP* STAT-KON* DEL139P is a compound based on Polycarbonate containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: Electrically Conductive, Exceptional Processing, Flame Retar..