Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.02 GPa | 1743 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON RX10409D PA 66 LNP* VERTON* RX10409D is a compound based on Nylon 66 containing proprietary fillers. Added feature of this grade is: Structural. |