Mechanical Properties Metric English Comments
Tensile Modulus 12.02 GPa
1743 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON RX10409D PA 66
LNP* VERTON* RX10409D is a compound based on Nylon 66 containing proprietary fillers. Added feature of this grade is: Structural.