Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.87 GPa | 1722 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP LX91475 PEEK LNP* LUBRICOMP* LX91475 is a compound based on Polyetheretherketone resin containing proprietary fillers. Added features of this material include: Easy Molding, High Temperature Bearing Grade, Wear.. |