Polymer Property : Tensile Modulus = 171 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.18 GPa
171 ksi
ASTM D638
Flint Hills 44S2A Polypropylene Impact Copolymer
Features: Phosphorus free additive package for silicon coated applications. Product does not contain animal derived components.Applications: Extrusion: blown and cast filmInformation Provided by Fl..
Tensile Modulus 1.18 GPa
171 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-LOY 63000CT PC+POLYESTER (Asia Pacific)
A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications
Tensile Modulus 1.18 GPa
171 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp TH0450D
LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by ..
Tensile Modulus 1.18 GPa
171 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific)
LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by ..
Tensile Modulus 1.18 GPa
171 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-LOY M3000C PP
LNP* STAT-LOY* M3000C is a compound based on unfilled Polypropylene resin. Added features of this grade include: Clean Compound System, Antistat.
Tensile Modulus 1.18 GPa
171 ksi
ASTM D 638
Saint-Gobain Meldin® 3110 Thermoplastic Bearing Material
3110 has a very low coefficient of friction and is particularly well suited for use with soft mating surface materials such as aluminum and soft stainless steel. Meldin® 3100 materials have exce..
Tensile Modulus 1.18 GPa
171 ksi
ISO 527
BASF Ultramid® HFX 35 PA6 (Dry)
Description: Ultramid HFX 35 is a polyamide specialty extrusion resin combining high flexibility, outstanding chemical resistance and enhanced heat stability.Applications: Ultramid HFX 35 is recomme..
Tensile Modulus 1.18 GPa
171 ksi
1 mm/min
Arkema Group Appryl® 3120 MU 5 Polypropylene - Polyethylene Copolymer
PP/PE copolymer Colored directly or during the injection molding process. This grade with a very good impact test, has been developed for interior trim automotive applications. It is UV stabilized.I..
Tensile Modulus 1.18 GPa
171 ksi
ISO 527-1/-2
DuPont Performance Polymers Hytrel® SC988 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
82 Shore D High Performance Polyester Elastomer Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers
Tensile Modulus 1.18 GPa

@Temperature 23.0 °C
171 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® SC988 NC010 TPC-ET  (Unverified Data**)
Hytrel® SC988 NC010 is the highest modulus grade, with nominal hardness of 82D, contains a non-discoloring stabilizer. Can be processed by various thermoplastic processing techniques. Developed for..