Material Notes:
Description: Ultramid HFX 35 is a polyamide specialty extrusion resin combining high flexibility, outstanding chemical resistance and enhanced heat stability.Applications: Ultramid HFX 35 is recommended for pipe and tubing applications requiring high melt strength and flexibility.Information provided by BASF
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.0 MPa
6960 psi
ISO 527
Elongation at Break 200 %
200 %
Nominal; ISO 527
Elongation at Yield 30 %
30 %
ISO 527
Tensile Modulus 1.18 GPa
171 ksi
ISO 527
Flexural Modulus 1.05 GPa
152 ksi
ISO 178
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C
118 °F
ISO 75
Processing Properties Metric English Comments
Zone 1 225 - 245 °C
437 - 473 °F
Rear
Zone 2 225 - 250 °C
437 - 482 °F
Middle
Zone 3 225 - 245 °C
437 - 473 °F
Front
Zone 4 230 - 245 °C
446 - 473 °F
Head
Zone 5 230 - 245 °C
446 - 473 °F
Flange
Die Temperature 230 - 245 °C
446 - 473 °F
Melt Temperature 225 - 245 °C
437 - 473 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
Commercial Status North America