Polymer Property : Tensile Modulus = 170.4 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.175 GPa
170.4 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 258 PA Black 2N PA66, DRY
Description: Unreinforced and modified polyamide 66, UV and thermal stabilized with excellent impact resistance, for injection molding.Available in: Europe Product Applications: TECHNYL® A 258P1 ..