Material Notes:
Description: Unreinforced and modified polyamide 66, UV and thermal stabilized with excellent impact resistance, for injection molding.Available in: Europe Product Applications: TECHNYL® A 258P1 BLACK 2N offers excellent impact resistance properties at ambient and low temperature and special low rigidity. This grade is commonly used for fasteners, cable ties and dowels. This product is available in black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 44.0 MPa
6380 psi
ISO 527 Type 1A
Elongation at Break 290 %
290 %
ISO 527 Type 1A
Tensile Modulus 1.175 GPa
170.4 ksi
ISO 527 Type 1A
Charpy Impact, Notched 1.17 J/cm²

@Temperature -30.0 °C
5.57 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
9.05 J/cm²

@Temperature 23.0 °C
43.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
1210
HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
1210
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
1210
Processing Properties Metric English Comments
Feed Temperature 260 - 270 °C
500 - 518 °F
Mold Temperature 50.0 °C
122 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 270-275°C