Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 17.58 GPa | 2550 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON RE0039 PA 66 LNP STAT-KON* RE0039 is a compound based on Nylon 66 resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |