Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 17.51 GPa | 2540 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Asia Pacific) LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Tensile Modulus | 17.51 GPa | 2540 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Europe-Africa-Middle East) LNP VERTON* RV00AES is a compound based on PA 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Tensile Modulus | 17.51 GPa | 2540 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |