Polymer Property : Tensile Modulus = 1690 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 11.7 GPa
1690 ksi
ASTM D638
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced
Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
Tensile Modulus 11.65 GPa
1690 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON EX99689C PEI
LNP* STAT-KON* EX99689C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Tensile Modulus 11.65 GPa
1690 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp EC002E PEI
LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas..
Tensile Modulus 11.65 GPa
1690 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp EC002E PEI (Asia Pacific)
LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac..
Tensile Modulus 11.65 GPa
1690 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp GF008 PSU
LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 11.65 GPa
1690 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Asia Pacific)
LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 11.65 GPa
1690 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Europe-Africa-Middle East)
LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.