Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 1664 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 11.47 GPa
1664 ksi
RT, Y direction; ASTM D638
Rogers Corporation RO4350B Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil
RO4000® Series High Frequency Circuit Materials are glass-reinforced hydrocarbon and ceramic (not PTFE) laminates with TICER™ TCR® Thin Film Resistor Foils. These laminates are designed for perf..
Copyright © lookpolymers.com All Rights Reserved