Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.47 GPa | 1664 ksi | RT, Y direction; ASTM D638 |
Rogers Corporation RO4350B Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil RO4000® Series High Frequency Circuit Materials are glass-reinforced hydrocarbon and ceramic (not PTFE) laminates with TICER™ TCR® Thin Film Resistor Foils. These laminates are designed for perf.. |