Polymer Property : Tensile Modulus = 1636 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 11.28 GPa
1636 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP RFL159 PA 66
LNP* LUBRICOMP* RFL159 is a compound based on Nylon 66 resin containing 25% Glass Fiber, 5% PTFE. Added features of this material include: Wear Resistant, Flame Retardant