Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.89 GPa | 1579 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DE004 PC LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 10.89 GPa | 1579 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DE004 PC (Asia Pacific) LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |