Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.4 GPa | 2090 ksi | ISO 527-2/1A/1 |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte.. |
|||
Tensile Modulus | 14.4 GPa | 2090 ksi | 1 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and .. |
|||
Tensile Modulus | 14.4 GPa | 2090 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP OF008 PPS - Linear (Europe-Africa-Middle East) LNP* Thermocomp* OF008 is a compound based on PPS - Linear resin containing Glass Fiber. |
|||
Tensile Modulus | 14.4 GPa | 2090 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP PX94085 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PX94085 is a compound based on PA6 resin, containing Glass Fiber. |
|||
Tensile Modulus | 14.4 GPa | 2090 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UF009AS PPA (Europe-Africa-Middle East) LNP* Thermocomp* UF009AS is a compound based on Polyphthalamide resin containing Glass Fiber. |
|||
Tensile Modulus | 14.4 GPa | 2090 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UF009AXP PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF009AXP is a compound based on Polyphthalamide resin containing 45% Glass Fiber. |
|||
Tensile Modulus | 14.4 GPa | 2090 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Verton OX07411 PPS (Asia Pacific) LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 14.4 GPa | 2090 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Verton OX07411 PPS LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |