Polymer Property : Tensile Modulus = 2090 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 14.4 GPa
2090 ksi
ISO 527-2/1A/1
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte..
Tensile Modulus 14.4 GPa
2090 ksi
1 mm/min, Type 1A; ISO 527-2
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and ..
Tensile Modulus 14.4 GPa
2090 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP OF008 PPS - Linear (Europe-Africa-Middle East)
LNP* Thermocomp* OF008 is a compound based on PPS - Linear resin containing Glass Fiber.
Tensile Modulus 14.4 GPa
2090 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP PX94085 PA 6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* PX94085 is a compound based on PA6 resin, containing Glass Fiber.
Tensile Modulus 14.4 GPa
2090 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP UF009AS PPA (Europe-Africa-Middle East)
LNP* Thermocomp* UF009AS is a compound based on Polyphthalamide resin containing Glass Fiber.
Tensile Modulus 14.4 GPa
2090 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP UF009AXP PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UF009AXP is a compound based on Polyphthalamide resin containing 45% Glass Fiber.
Tensile Modulus 14.4 GPa
2090 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Verton OX07411 PPS (Asia Pacific)
LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 14.4 GPa
2090 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Verton OX07411 PPS
LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.