Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.950 GPa | 138 ksi | |
Plastcom SLOVALEN PQ 91T 5 PP, 5% mineral filling FeaturesModified PP for injection moulding with the content of 5 % mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Tensile Modulus | 0.950 GPa | 138 ksi | |
Plastcom SLOVAMID 66 SHI PA66, improved strength Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Tensile Modulus | 0.950 GPa | 138 ksi | ISO 527 |
Quadrant EPP Cestilene™ HD 1000 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Tensile Modulus | >= 0.950 GPa | >= 138 ksi | 1 mm/min; ISO 527 |
MTM Plastics Dipolen® H Recycled HDPE Blend Dipolen® H is a granulated HDPE with other polyolefin blend for use in either extrusion or injection molding. It can be supplied unmodified or treated with additives according to customer specif.. |
|||
Tensile Modulus | 0.950 GPa | 138 ksi | 1mm/min; ISO 527-2 |
Borealis EE002AE Polypropylene Elastomer Modified EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties.. |
|||
Tensile Modulus | 0.950 GPa | 138 ksi | 1mm/min; ISO 527-2 |
Borealis MG7547B Polyethylene MG7547B is a high-density polyethylene produced by a low pressure process. This grade has an excellent impact strength and low distortion even at low temperatures. It also contains UV stabilizer, wh.. |
|||
Tensile Modulus | 0.950 GPa | 138 ksi | 1mm/min; ISO 527-2 |
Borealis MG7547S Polyethylene MG7547S is a high-density polyethylene produced by a low pressure process. This grade has an excellent impact strength and low distortion even at low temperatures. It also contains UV stabilizer, wh.. |
|||
Tensile Modulus | 0.950 GPa | 138 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4155 black 9992 PA612-I Information provided by EMS Grivory |
|||
Tensile Modulus | 0.951 GPa | 138 ksi | ISO527-2/1 |
ExxonMobil PP8013L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with very high impact strength at low temperature. It is suitable for molding applications like containers and tubs, other rigid packaging, t.. |
|||
Tensile Modulus | 0.950 GPa | 138 ksi | ISO 527-2 |
Domo 2600TC Polypropylene Copolymer Information provided by Domo. |
|||
Tensile Modulus | 0.950 GPa | 138 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. .. |
|||
Tensile Modulus | 0.950 GPa | 138 ksi | |
BASF Novolen® 2600 TC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 0.951 GPa | 138 ksi | ASTM D638 |
Ravago Manufacturing Americas Echo® RPPC 20/2 BK Recycled Polypropylene Copolymer Polypropylene, Unreinforced, 20 MFI, 2 Izod, BlackEntecs proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, .. |
|||
Tensile Modulus | 0.950 GPa | 138 ksi | ASTM D638 |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 0.950 GPa | 138 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BRZ 334 H PA6 Product description: Grilon BRZ 334 H is a heat stabilized, medium viscosity, high impact modified PA6 extrusion grade. Grilon BRZ 334 H has the following important properties:High impact strength a.. |