Polymer Property : Tensile Modulus = 13.82 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 13.82 GPa
2004 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6
LNP* Konduit* PX08321 a compound based on PA6 resins containing mineral. Added features include: Thermally Conductive.
Tensile Modulus 13.82 GPa
2004 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 compound