Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.03 GPa | 1890 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP LF006E PEEK LNP* THERMOCOMP* LF006E is a compound based on Polyetheretherketone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Tensile Modulus | 13.03 GPa | 1890 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF008ESY PA 66 LNP THERMOCOMP* RF008ESY is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Tensile Modulus | 13.03 GPa | 1890 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RX00713H PA 66 LNP* Thermocomp* RX00713H is a compound based on Nylon 6/6 containing proprietary fillers. Characteristics of this grade are: Healthcare. |