Polymer Property : Tensile Modulus = 127 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.875 GPa
127 ksi
ISO 527-1/-2
Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data)
Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su..
Tensile Modulus 0.875 GPa
127 ksi
1mm/min; ISO 527
BASF Ultramid® 8254 HS BK-102 PA6 (Dry)
Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications.