Mechanical Properties Metric English Comments
Tensile Modulus 12.42 GPa
1801 ksi
ASTM D638
Plenco 51240 PET, Pellet, Injection Molded, Green  (discontinued **)
PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P..
Tensile Modulus 12.42 GPa
1801 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP QF008 PA 6/10 (Asia Pacific)
LNP* Thermocomp* QF008 is a compound based on Nylon 6/10 resin containing Glass Fiber.
Tensile Modulus 12.42 GPa
1801 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP QF008 PA6.10
LNP* THERMOCOMP* QF008 is a compound based on Nylon 6/10 resin containing 40% Glass Fiber.
Tensile Modulus 12.42 GPa
1801 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp QF008R PA 6/10
LNP* Thermocomp* QF008R is a compound based on Nylon 6/10 containing Glass Fiber. Characteristics of this grade are: Easy Release.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 12.42 GPa
1801 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp QF008S PA 6/10
LNP* Thermocomp* QF008S is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas ..
Tensile Modulus 12.42 GPa
1801 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RX10408H PA 66
LNP* Thermocomp* RX10408H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare.
Tensile Modulus 12.42 GPa
1801 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp QF008S PA 6/10 (Asia Pacific)
LNP* Thermocomp* QF008S is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci..