Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.787 GPa @Temperature -50.0 °C |
1129 ksi @Temperature -58.0 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |