Mechanical Properties Metric English Comments
Tensile Modulus 0.0800 GPa
11.6 ksi
1 mm/min; ASTM D638 - ISO 527-2
DuPont Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer
Elvaloy® 1209 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Tensile Modulus 0.0800 GPa
11.6 ksi
1 mm/min; ASTM D638 - ISO 527-2
DuPont Elvaloy® 1609 AC Ethylene and 9% Methyl Acrylate Copolymer
Elvaloy® 1609 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Tensile Modulus 0.0800 GPa
11.6 ksi
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8341G BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Slightly Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Modulus 0.0800 GPa
11.6 ksi
1 mm/min
Arkema Group Evatane® 1003 VN 4 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for transparent and thermal agricultural film for greenhouse coverage.ISO data provided by the manufacturer, Arkema.
Tensile Modulus >= 0.0800 GPa
>= 11.6 ksi
in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam
AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable..
Tensile Modulus >= 0.0800 GPa
>= 11.6 ksi
perpendicular to plane; ASTM C297
3A Composites Core Materials AIREX® T92.80 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r..