Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0800 GPa | 11.6 ksi | 1 mm/min; ASTM D638 - ISO 527-2 |
DuPont Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1209 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Tensile Modulus | 0.0800 GPa | 11.6 ksi | 1 mm/min; ASTM D638 - ISO 527-2 |
DuPont Elvaloy® 1609 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1609 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Tensile Modulus | 0.0800 GPa | 11.6 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8341G BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Slightly Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 0.0800 GPa | 11.6 ksi | 1 mm/min |
Arkema Group Evatane® 1003 VN 4 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for transparent and thermal agricultural film for greenhouse coverage.ISO data provided by the manufacturer, Arkema. |
|||
Tensile Modulus | >= 0.0800 GPa | >= 11.6 ksi | in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |
|||
Tensile Modulus | >= 0.0800 GPa | >= 11.6 ksi | perpendicular to plane; ASTM C297 |
3A Composites Core Materials AIREX® T92.80 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r.. |