Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.50 - 11.5 GPa | 1380 - 1670 ksi | ISO 527 |
Vyncolit X681 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica.. |
|||
Tensile Modulus | 9.50 - 11.5 GPa | 1380 - 1670 ksi | ISO 527 |
Vyncolit 2950 W Novolac Phenolic Mineral and glass fiber filled phenolic molding compound with a very high strain to failure in flexure. UL listed.USES: Armature insulation.Information provided by Vyncolit, a Sumitomo Bak Group |