Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.21 GPa | 1626 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RX06480 PA 66 LNP LUBRICOMP* RX06480 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% Lubricants. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 11.21 GPa | 1626 ksi | ASTM D638 |
Plenco 50240 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black.. |