Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 70.0 GPa | 10200 ksi | Young's; DINV ENV 843-2 / ASTM-F417 |
CeramTec Sikor® E Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Tensile Modulus | 70.0 GPa | 10200 ksi | Young's; DINV ENV 843-2 / ASTM-F417 |
CeramTec Sikor® S Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Tensile Modulus | 70.0 GPa | 10200 ksi | Longitudinal |
Goodfellow Carbon/Epoxy Composite Sheet Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow. |
|||
Tensile Modulus | 70.0 GPa @Temperature 175 °C |
10200 ksi @Temperature 347 °F |
Material as cured |
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix 5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel |
|||
Tensile Modulus | 70.0 GPa | 10200 ksi | 0° |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, High Strength 6k carbon Balanced fabric 285 g/m2 Information provided by HexCel |
|||
Tensile Modulus | 70.3 GPa | 10200 ksi | |
DuPont™ Kevlar® 29 Aramid Fiber 1500 Denier; 1000 Filaments. Kevlar® 29 yarns are used in ballistic applications, ropes and cables, protective apparel such as cut-resistant gloves, in life protection uses such as helmets, vehicu.. |
|||
Tensile Modulus | 70.0 GPa | 10200 ksi | |
COI Ceramics Nextel™ A-N720 Oxide Ceramic Matrix Composite, Alumina Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |