Polymer Property : Tensile Modulus = 10.73 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 10.73 GPa
1556 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF006SXZ PA 66
LNP* THERMOCOMP* RF006SXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this material is: Heat Stabilized.