Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.64 GPa | 1543 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc.. |
|||
Tensile Modulus | 10.64 GPa | 1543 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FR50 BK505 Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 BK505 is a 25% glass fiber reinforced flame retardant black polyamide 66 resin for injection molding.Information provided by DuPont Perfo.. |