DuPont Performance Polymers Zytel® FR50 BK505 Nylon 66  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® FR50 BK505 Nylon 66  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zytel® FR50 BK505 is a 25% glass fiber reinforced, flame retardant black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers