Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.41 GPa | 1510 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6 (Asia Pacific) LNP* Thermocomp* PF006U is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: UV Stabilized. |
|||
Tensile Modulus | 10.41 GPa | 1510 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF006I PA 66 LNP* THERMOTUF* RF006I is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: High Impact. |
|||
Tensile Modulus | 10.41 GPa | 1510 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOTUF RF006I PA 66 LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Tensile Modulus | 10.41 GPa | 1510 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermotuf RF006I PA 66 LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas region... |