Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* PF006U is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: UV Stabilized.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 158 MPa
22900 psi
ASTM D638
Elongation at Break 2.8 %
2.8 %
ASTM D638
Tensile Modulus 10.41 GPa
1510 ksi
50 mm/min; ASTM D638
Flexural Strength 255 MPa
37000 psi
ASTM D790
Flexural Modulus 8.96 GPa
1300 ksi
ASTM D790
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
Izod Impact, Unnotched 10.68 J/cm
20.01 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 202 °C

@Thickness 3.20 mm
396 °F

@Thickness 0.126 in
unannealed; ASTM D648
Copyright © lookpolymers.com All Rights Reserved