Polymer Property : Tensile Modulus = 1.700 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accucomp ABS ABS846HL High Flow Medium Impact Grade
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accucomp ABS ABS892BL High Heat Grade
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accuguard ABS ABS860V0L Flame Retardant
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Acculoy POL063L Polycarbonate PET Alloy
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0437G10CL Glass Reinforced Coupled
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0437M20CL Mica Reinforced Coupled
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0437T30L1 Talc Reinforced
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer HP0334W10L Wollastonite Reinforced
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0334C20L Calcium Reinforced
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0334C30L1 Calcium Reinforced
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0334T10L Talc Reinforced
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0334T20L1 Talc Reinforced
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0336T20L1 Talc Reinforced
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0336W10L Wollastonite Reinforced
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0339C20L Calcium Reinforced
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Acculoy PCA083L Polycarbonate ABS Alloy
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Acculoy POL062L Polycarbonate PET Alloy
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0436W20L Wollastonite Reinforced
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0339T10L Talc Reinforced
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0339W10L Wollastonite Reinforced