Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.445 GPa @Temperature 120 °C |
209.6 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Dry) Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the.. |