Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.009873 GPa | 1.432 ksi | Storage |
Epoxy Technology EPO-TEK® T7109-18 Electrically Insulating Epoxy Paste Material Description: A flexible, electrically insulating epoxy paste designed for low stress and heat dissipation applications. Alternative to EPO-TEK® T7109-17.Information Provided by Epoxy Tec.. |