Polymer Property : Tensile Modulus = 0.009873 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.009873 GPa
1.432 ksi
Storage
Epoxy Technology EPO-TEK® T7109-18 Electrically Insulating Epoxy Paste
Material Description: A flexible, electrically insulating epoxy paste designed for low stress and heat dissipation applications. Alternative to EPO-TEK® T7109-17.Information Provided by Epoxy Tec..