Polymer Property : Tensile Modulus = 0.7750 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.7750 GPa
112.4 ksi
ASTM D638
3D Systems VisiJet M100 3-D Printer Model Material
The InVision SR (standard resolution) 3-D printer delivers key advantages compared to other 3-D modeling technologies — superior model quality, durable photopolymer materials, surface finish and fe..