Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.540 GPa | 78.3 ksi | 1 mm/min |
Arkema Group Rilsan® BMN P20 D Nylon 11 (Dry) Designation ISO 1874-PA11-P,MR,12-004Flexible grade for injection molding. Available colors: black and natural. Mold release agent.Outstanding working properties. Easy filling of the mold due to its.. |
|||
Tensile Modulus | 0.540 GPa | 78.3 ksi | TD; ASTM D882-A |
Borealis Borstar® FB4370 Medium Density Polyethylene Borstar® FB4370 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Applications: Borstar® FB4370 has been developed especially for ap.. |