Arkema Group Rilsan® BMN P20 D Nylon 11 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Unreinforced
Manufacturer Arkema
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® BMN P20 D Nylon 11 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA11-P,MR,12-004Flexible grade for injection molding. Available colors: black and natural. Mold release agent.Outstanding working properties. Easy filling of the mold due to its well adapted melt viscosity. Low shrinkage: include 1% on average for the design of the mold. Good dimensional stability (low moisture absorption).UL classification: UL94 HB RTI(C) 65/65/65Example applications: Flexible mechanical parts with impact and vibrations resistance.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Water Absorption 1.8 %
1.8 %
Melt Flow 18.3 g/10 min

@Load 2.16 kg,
Temperature 235 °C
18.3 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 35 %
35 %
50 mm/min
Tensile Modulus 0.540 GPa
78.3 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 1.90 J/cm²
9.04 ft-lb/in²
0.520 J/cm²

@Temperature -30.0 °C
2.47 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 183 °C
361 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.10 mm
HB

@Thickness 0.122 in
Electrical Properties Metric English Comments
Dissipation Factor 0.000347

@Frequency 1e+6 Hz
0.000347

@Frequency 1e+6 Hz
0.000708

@Frequency 100 Hz
0.000708

@Frequency 100 Hz