Polymer Property : Tensile Modulus = 0.485 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.485 GPa

@Temperature 80.0 °C
70.3 ksi

@Temperature 176 °F
ISO Data
BASF Ultramid® 8202 HS PA6 (Dry)
Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab..
Tensile Modulus 0.485 GPa

@Temperature 80.0 °C
70.3 ksi

@Temperature 176 °F
ISO Data
BASF Ultramid® 8202 PA6 (Dry)
Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult..